Wide-angle optics
Broadband antireflection from 0° to 30°
AstraLayer 2.18
Specification
Minimize front-surface reflectance from 420 to 680 nm for unpolarized light incident from air. Optimize one coating against five spectra, at 0°, 7.5°, 15°, 22.5° and 30°.
8layers
0.0884 ppjoint RMS error
0.338%maximum reflectance
Calculated result
The largest residual reflection occurs at 680 nm and 30°. At normal incidence the peak shifts to the opposite edge of the band, 420 nm, where reflectance reaches 0.236%.
Materials, layer recipe and calculation settings
TiO₂ and MgF₂ films on N-BK7. Each curve is the mean of s- and p-polarized reflectance at one angle. The film models use the dispersions of Siefke et al. (TiO₂, 2016) and Franta et al. (MgF₂, 2017).
Select “AR 0–30°” and set both films and the substrate to Complex. The Verification worksheet lists all five spectra on the same 2,001-wavelength grid. The joint RMS is the root mean square of the reflectance errors across wavelengths and angles.
Laser optics
A dual-band mirror for 532 and 1064 nm
AstraLayer 2.18
Specification
Reflect in two bands around the laser lines, 510–555 nm and 1020–1110 nm. Between them, suppress reflection from 640 to 900 nm. The transition regions have no reflectance target.
98.149%minimum R · 510–555 nm
0.599%maximum R · 640–900 nm
99.098%minimum R · 1020–1110 nm
Calculated result
The 35-layer design keeps reflectance below 0.60% throughout the central window. The shaded regions mark the three specified bands. The dashed segments show their targets.
Materials, layer recipe and calculation settings
Ta₂O₅ and SiO₂ films on N-BK7 at normal incidence. Both films use wavelength-dependent optical constants from Franta et al. (Ta₂O₅, 2015 and SiO₂, 2016). The glass uses the N-BK7 library profile.
Select “Dual-band mirror 532 & 1064 nm” and set both films and the substrate to Complex. The Design worksheet lists every layer. The Verification worksheet gives the response on a 2,013-wavelength grid.
Ultrafast optics
A chirped mirror for pulse compression
AstraLayer 2.18
Specification
Hold group-delay dispersion (GDD) at −50 ± 20 fs² from 700 to 900 nm while keeping reflectance at or above 99.5%. The two targets apply to the same mirror at every wavelength.
37layers
99.663%minimum reflectance
19.3 fs²maximum GDD error
Calculated result
All 2,001 wavelengths on the independent verification grid meet both targets. In the lower plot, the shaded region is the allowed GDD interval and the dashed line marks −50 fs².
Materials, layer recipe and calculation settings
TiO₂ / SiO₂ on fused silica, at normal incidence. The calculation uses wavelength-dependent film profiles from Siefke et al. (TiO₂, 2016) and Franta et al. (SiO₂ and fused silica, 2016).
Reproduce with “Dispersive mirror, Complex”. The starting design has 12 chirped pairs. The Verification sheet contains both spectra on the dense grid.
Colorimetry
An amber filter specified in CIE xyY
AstraLayer 2.18
Specification
Target amber in transmission under D65 illumination for the CIE 2° standard observer. Specify chromaticity x = 0.580 and y = 0.414, with relative luminance Y = 44%. Leave 520–600 nm free for the filter edge.
0.5812achieved x
0.4129achieved y
45.51%achieved Y
Calculated result
The 20-layer filter reaches x = 0.5812 and y = 0.4129. Its chromaticity error is 0.0016 against a tolerance of 0.010. Relative luminance is 45.51%, within the specified 44% ± 5 percentage points.
Materials, layer recipe and calculation settings
TiO₂ / SiO₂ on N-BK7. Both films use the Siefke and Franta thin-film profiles. The substrate uses the library N-BK7 profile.
Start from “Dichroic amber filter” and set both layer materials and the substrate to Complex. See Color for the target and achieved xyY, and Materials for sampled n and k.
Chromaticity field adapted from the CIE 1931 2° observer data · CC BY-SA 4.0.
Multiple substrates
Two plates, one transmission target
AstraLayer 2.18
Specification
A sapphire protective window sits in front of an N-BK7 plate with an air gap. Optimize all four coated faces for transmission through the complete assembly over 420–680 nm.
4coated faces
24layers in total
98.575%minimum assembly T
Calculated result
Six layers are deposited on each face. The internal reflections of the thick media are combined by intensity. The plotted spectrum therefore includes both plates and the air gap.
Materials, layer recipe and calculation settings
TiO₂ and MgF₂ films coat the sapphire and N-BK7 plates. The sapphire model uses the ordinary refractive index reported by Malitson and Dodge. Film dispersions are from Siefke et al. (TiO₂, 2016) and Franta et al. (MgF₂, 2017).
Run “Air-spaced pair, four AR coatings” with its defaults. C1 and C2 are deposited on sapphire, C3 and C4 on N-BK7. The Design sheet gives a separate layer recipe for every face.
High-power laser optics
A 1030 nm mirror with a field limit in Ta₂O₅
AstraLayer 2.18
Specification
Reflect at least 99.9% from 960 to 1100 nm. At the laser wavelength of 1030 nm, keep the normalized electric-field intensity |E|²/|E₀|² in every Ta₂O₅ layer at or below 40%.
38.44%peak in Ta₂O₅
40%Ta₂O₅ field limit
99.954%minimum reflectance
Calculated result
At 1030 nm the peak in Ta₂O₅ is 38.44% of the incident field intensity, below the 40% limit. The largest antinodes lie in SiO₂. Across the design band the mirror reflects at least 99.954%.
Materials, layer recipe and calculation settings
Ta₂O₅ / SiO₂ on fused silica. Dispersive profiles from Franta et al. are used for tantala (2015), silica film (2016) and substrate (2016). Normal incidence, s-polarized field.
Select “High-power HR mirror 1030 nm” and switch both films and the substrate to Complex. The Field sheet gives the full depth profile and the peak in each layer of the 41-layer design.
Double-sided optics
Antireflection on both faces of a window
AstraLayer 2.18
Specification
Maximize transmittance through a plane-parallel N-BK7 window from 420 to 680 nm. Vary the front and rear coatings independently while optimizing the transmittance of the complete window.
6 + 6front + rear layers
99.535%minimum window T
0.144 ppdense-grid RMS
Calculated result
Across the verification grid, the complete coated window transmits 99.535–99.996% at normal incidence. The workbook lists both six-layer recipes with their respective thicknesses.
Materials, layer recipe and calculation settings
The TiO₂ and MgF₂ films use the dispersions of Siefke et al. (2016) and Franta et al. (2017), respectively. The glass uses the N-BK7 library profile. Both exterior media are air.
Choose “Window, AR both sides” and set the high-index film, low-index film and substrate to Complex. Both faces remain synthesized in the stack editor.